| Ukwakheka kwamakhemikhali | ||||||||
| Ibanga | Ti | Al | V | UFe, ubuningi | C, ubuningi | N, ubuningi | H, ubuningi | O, ubuningi |
| I-Ti-6Al-4V ELI | I-Bal | 5.5~6.5 | 3.5~4.5 | 0.25 | 0.08 | 0.05 | 0.012 | 0.13 |
| Ibanga lesi-5 (Ti-6Al-4V) | I-Bal | 5.5~6.75 | 3.5~4.5 | 0.3 | 0.08 | 0.05 | 0.015 | 0.2 |
| Izakhiwo zemishini | |||||
| Ibanga | Isimo | Amandla Okudonsa (Rm/Mpa) ≥ | Amandla Okukhiqiza (Rp0.2/Mpa) ≥ | Ukwelulwa (A%) ≥ | Ukunciphisa Indawo (Z%) ≥ |
| I-Ti-6Al-4V ELI | M | 860 | 795 | 10 | 25 |
| Ibanga lesi-5 (Ti-6Al-4V) | M | 860 | 780 | 10 | / |
Isakhiwo esincane se-titanium bars se-XINNUO esikhiqizwe yi-Ti-6Al-4V ELI singafinyelela ngaphakathi kwe-A3 kanti i-Tensile Strength ingafinyelela ngaphezu kwe-1100Mpa. I-titanium bar yezikulufo zomgogodla isetshenziselwa ukufakwa komgogodla, ikhwalithi ibaluleke kakhulu.
1. Ukwakheka kwamakhemikhali kunqunywa yizinga lesiponji se-titanium elisetshenzisiwe, i-XINNUO isebenzisa okusanhlamvu okungaphansi kwebanga le-O;
2. Isakhiwo esincane sinqunywa ngezikhathi zokuncibilika, i-XINNUO incibilika izikhathi ezi-3 nge-oven yaseJalimane i-ALD engenisiwe;
3. Izakhiwo zemishini zinqunywa yizinqubo zokugoqa nokufaka, i-XINNUO ilawula zonke izinyathelo zokukhiqiza;
4. Amaphutha angaphakathi kanye nokuqhekeka kobuso kunqunywa ukuhlolwa kwekhwalithi, i-XINNUO isebenzisa i-Eddy current flaw detector kanye ne-Ultrasonic flaw detector ukuhlola yonke ibha;
5. Ubuso be-XINNUO titanium bars buhlolwa yi-ODE optical surface detector ehlanganisa ukutholwa ngesandla;
6. Ukubekezelela imigoqo ye-titanium ye-XINNUO kuhlolwa ngesilinganiso sobubanzi be-Infra-ray.
Zonke lezi zinqubo ziholela ekhwalithini yokugcina yamabha e-titanium ezokwelapha futhi zaqinisekisa ikhwalithi yemikhiqizo ye-XINNUO.